REXPEARL EEA:A1100、A3100、A1150、A4200、A6200、A4250
| Typical Properties | Unit | Test Method | 
| Melt Flow Rate | g/10min | ISO 1872-2 | 
| EA Content | wt% | JPE Method | 
| Tensile Modulus | MPa | ISO 1872-2 | 
| Tensile Strength at Yield | MPa | ISO 1872-2 | 
| Tensile Strength at Break | MPa | ISO 1872-2 | 
| Tensile Strain at Break | % | ISO 1872-2 | 
| Flexural Modulus | MPa | ISO 1872-2 | 
| Charpy Impact Strength | kJ/m2 | ISO 1872-2 | 
| Tensile Impact Strength | kJ/m2 | ISO 1872-2 | 
| Durometer Hardness(Type-D) | - | ISO 868 | 
| Vicat Softening Point | ℃ | ISO 306 | 
| Melting Point | ℃ | ISO 11357-3 | 
| Brittleness Temperature | ℃ | ISO 974 | 
| Preparation Test Specimens | ||
| Uses | Film | |
| Sheet | ||
| Extrusion,Wire-Coating | ||
| Injection | ||
	
	
	 
| A1100 | A3100 | A1150 | A4200 | A6200 | A4250 | 
| 0.4 | 3 | 0.8 | 5 | 20 | 5 | 
| 10 | 10 | 15 | 20 | 20 | 25 | 
| 90 | 80 | 46 | 23 | 18 | - | 
| No-Yield | No-Yield | No-Yield | No-Yield | No-Yield | No-Yield | 
| No-Break | No-Break | No-Break | No-Break | No-Break | No-Break | 
| >400 | >400 | >400 | >400 | >400 | >400 | 
| 99 | 93 | 54 | 28 | 22 | 21 | 
| No-Break | No-Break | No-Break | No-Break | No-Break | No-Break | 
| 290 | 250 | 250 | 280 | 230 | 290 | 
| 46 | 44 | 41 | 34 | 31 | 30 | 
| 83 | 75 | 67 | 50 | 43 | 41 | 
| 104 | 104 | 100 | 96 | 94 | 92 | 
| <-70 | <-70 | <-70 | <-70 | <-70 | <-70 | 
| Compression | Compression | Compression | Compression | Compression | Compression | 
| ○ | ○ | ||||
| ○ | ○ | ○ | |||
| ○ | ○ | ○ | ○ | ○ | |
| ○ | 



 
			 
			 
			 
 
 
.jpg)